Linear Mold Shrinkage, Flow 0.0096 cm/cm

@Thickness 3.20 mm
0.0096 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® EX7631T PC
EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion.