Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0077 cm/cm | 0.0077 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP WAL34I PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WAL34I is a compound based on Polybutylene Terephalate resin containing PTFE, Aramid Fiber. Added features include Internally Lubricated. |