Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0063 cm/cm | 0.0063 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |