Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0058 cm/cm @Thickness 3.18 mm |
0.0058 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Linear Mold Shrinkage, Flow | 0.0058 cm/cm @Thickness 3.18 mm |
0.0058 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® XT X XT 1000 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Linear Mold Shrinkage, Flow | 0.0058 cm/cm | 0.0058 in/in | SABIC Method |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |