Polymer Property : Linear Mold Shrinkage, Flow = 0.0052 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0034 - 0.0052 cm/cm

@Thickness 3.20 mm
0.0034 - 0.0052 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Linear Mold Shrinkage, Flow 0.0034 - 0.0052 cm/cm

@Thickness 3.20 mm
0.0034 - 0.0052 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Linear Mold Shrinkage, Flow 0.0034 - 0.0052 cm/cm

@Thickness 3.20 mm
0.0034 - 0.0052 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS
PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr..