Polymer Property : Linear Mold Shrinkage, Flow = 0.0041 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0041 cm/cm
0.0041 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific)
LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat.
Linear Mold Shrinkage, Flow 0.0041 cm/cm
0.0041 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Linear Mold Shrinkage, Flow 0.0041 cm/cm
0.0041 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Linear Mold Shrinkage, Flow 0.0041 cm/cm
0.0041 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Linear Mold Shrinkage, Flow 0.0041 cm/cm
0.0041 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Linear Mold Shrinkage, Flow 0.0041 cm/cm
0.0041 in/in
ISO 294
BASF Ultradur S 4090 G4 High Speed Unc. 20% Glass Filled PBT
Ultradur S 4090 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled injection molding PBT for industrial parts, rigid tough and dimensional stable applications.