Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0038 cm/cm | 0.0038 in/in | SABIC Method |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm | 0.0038 in/in | 60x60x2; 300°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm | 0.0038 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX03633C PC LNP STAT-KON* DX03633C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0038 cm/cm | 0.0038 in/in | GB/T 15585-1995 |
Sichuan Deyang Haton® hXGR41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |