Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00300 cm/cm

@Thickness 3.17 mm
0.00300 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced
Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy. Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural off-whit..
Linear Mold Shrinkage, Flow 0.00300 cm/cm

@Thickness 3.17 mm
0.00300 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers PEI 30GF-Natural PEI, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristic..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
Injection; ISO 2577
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
Linear Mold Shrinkage, Flow 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
ASTM D955
Celanese CELANEX 1632Z PBT, 15% Glass Reinforced
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
ISO 294-4
Celanese CELANEX 3300 PBT, 30% Glass Reinforced
Ceanex 3300 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outstandi..
Linear Mold Shrinkage, Flow 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
ISO 294-4
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Celanese CELANEX 3300FC PBT, 30% Glass Reinforced
Celanex 3300FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Linear Mold Shrinkage, Flow 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
ISO 294-4
Celanese CELANEX 3300FC PBT, 30% Glass Reinforced
Celanex 3300FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ISO 294-4
Celanese CELANEX 3309HRLM PBT, 30% Glass Reinforced
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. lIt is a asermarkable ..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Celanese CELANEX 3400 PBT, 40% Glass Reinforced
Celanex 3400 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding p..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Celanese CELANEX 4300 PBT, 30% Glass Reinforced
Celanex 4300 is a toughened, 30% glass reinforced PBT.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ISO 294-4
Celanese CELANEX 4300LM PBT, 30% Glass Reinforced
Celanex 4300LM is a toughened 30% glass reinforced PBT that is enhanced for improved laser marking graphics.it is a lasermarkable grade available in a black color to mark white, The grade is special..
Linear Mold Shrinkage, Flow 0.00300 - 0.00600 cm/cm
0.00300 - 0.00600 in/in
ISO 294-4
Celanese CELANEX 4309AR PBT
Celanex 4309AR is a 30% glass reinforced PBT with enhanced resistance to hydrolysis, alkaline environments and salt water spray.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ISO 294-4
Celanese CELANEX 5300-2 PBT, 30% Glass Reinforced
Celanex 5300-2 is a 30% fiberglass reinforced polyester with improved surface finish. Celanex 5300-2 contains an internal lubricant.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Celanese CELANEX 5300-2 PBT, 30% Glass Reinforced
Celanex 5300-2 is a 30% fiberglass reinforced polyester with improved surface finish. Celanex 5300-2 contains an internal lubricant.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ASTM D955
Celanese Celstran® PP-GF20-02 AD 3002 PP, 20% Glass Reinforced
Celstran PP-Gf20-02 is a 20% long glass fiber Polypropylene. This material imparts excellent impact and modulus properties that exceed that short fiber polyproylene.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ASTM D955
Celanese Celstran® PPS-AF35-01- PPS, 35% Aramid Reinforced
PPS with 35% aramid fiber by weightInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 - 0.00600 cm/cm
0.00300 - 0.00600 in/in
ISO 294-4
Celanese FORTRON 1120L4 PPS, 20% Specialty
Fortron 1120L4 is a 20% glass fiber reinforced injection molding grade exhibiting excellent heat and chemical resistance, inherent flame retardancy, high hardness and stiffness at elevated temperatu..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Fortron 1130L4 is a 30% glass-reinforced PPS that has excellent heat and chemical resistance. It is inherently flame-retardant and exhibits high hardness and a good balance of strength and stiffness..
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ISO 294-4
Celanese THERMX LED 0201 PCT, 40% Specialty
Thermx LED 0201 is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low moist..
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ISO 294-4
Celanese THERMX TE4004 PCT, 40% Specialty
Thermx« TE4004 NC010 is a 40% glass fiber/glass flake reinforced polycyclohexylenedimethylene terephthalate resin developed for automotive ignition systems applications. PRELIMINARY DATAInformation..
Linear Mold Shrinkage, Flow 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
ISO 294-4
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ISO 294-4
Celanese THERMX CGT33 PCT, 30% Specialty
Thermx« CGT33 is a 30% glass fiber reinforced and toughened polycyclohexylenedimethylene terephthalate for injection molding.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ISO 294-4
Celanese THERMX LED 0201S PCT, 38% Specialty
Thermx LED 0201S is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low mois..
Linear Mold Shrinkage, Flow 0.00300 - 0.00400 cm/cm
0.00300 - 0.00400 in/in
Injection; ISO 2577
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ISO 294-4
Celanese FORTRON 6345L4 PPS, 30% Specialty
Fortron 6345L4 is 30% glass fiber/high PTFE reinforced injection molding grade. This grade, available in natural and black color, exhibits improved wear and sliding properties versus 1342L4 product...
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ISO 294-4
Celanese Hostaform® C 9021 GV1/30 GT POM, 26% Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 cm/cm
0.00300 in/in
ASTM D955
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ISO 294-4
Celanese CELANEX 4302LM PBT, 30% Glass Reinforced
Celanex 4302LM is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.Information provided b..
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ASTM D955
Celanese VANDAR 4662Z PBT, 30% Glass Reinforced
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..