Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00141 cm/cm
0.00141 in/in
ISO 294-4, 2577
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified