Polymer Property : Linear Mold Shrinkage, Flow = 0.00124 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00124 cm/cm
0.00124 in/in
ISO 294-4, 2577
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber
PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance