Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00080 - 0.0010 cm/cm @Time 86400 sec |
0.00080 - 0.0010 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.00080 - 0.0018 cm/cm @Thickness 3.20 mm |
0.00080 - 0.0018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Linear Mold Shrinkage, Flow | 0.00080 - 0.0028 cm/cm @Time 86400 sec |
0.00080 - 0.0028 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.00080 - 0.0010 cm/cm @Time 86400 sec |
0.00080 - 0.0010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | >= 0.00080 cm/cm | >= 0.00080 in/in | on Tensile Bar; E2P method |
Eurostar Staramide ACF6 PA66, 30% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF6 is a 30% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |