Polymer Property : Linear Mold Shrinkage, Flow = 0.000090 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.000090 cm/cm
0.000090 in/in
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491..