Physical Properties | Metric | English | Comments |
---|---|---|---|
c Lattice Constant | 6.29 Ã… | 6.29 Ã… | |
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal Large birefringence and wide transparency range (400 to 4000 nm); finds uses as fiber optic isolators, circulators, and beam displacers. Grown by Czochralski method.Data provided by the supplier, M.. |