Physical Properties | Metric | English | Comments |
---|---|---|---|
c Lattice Constant | 6.26 Ã… | 6.26 Ã… | |
MarkeTech Lithium Aluminum Oxide (LiAlO2) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.4%. |
|||
c Lattice Constant | 6.26 Ã… | 6.26 Ã… | |
Mateck LiAlO2 Substrate single crystals for III-V nitrides |