Physical Properties | Metric | English | Comments |
---|---|---|---|
c Lattice Constant | 3.42 Ã… | 3.42 Ã… | C/2 |
Momentive Performance Materials "PG" Pyrolytic Graphite Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne.. |