Physical Properties | Metric | English | Comments |
---|---|---|---|
c Lattice Constant | 12.63 Ã… | 12.63 Ã… | |
MarkeTech Strontium Lanthanum Aluminate (SrLaAlO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
c Lattice Constant | 12.63 Ã… | 12.63 Ã… | |
Mateck SrLaAlO4 Substrate single crystals for superconductivity |