Polymer Property : Specific Gravity = 2.191 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.191 - 2.224 g/cc

@Thickness 0.762 mm
2.191 - 2.224 g/cc

@Thickness 0.0300 in
Fiberglass Reinforced
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements
GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and..