Specific Gravity 1.62 - 1.66 g/cc

@Thickness 0.508 mm
1.62 - 1.66 g/cc

@Thickness 0.0200 in
Aramid/Glass
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements
GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and..