Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.055 g/cc @Temperature 25.0 °C |
1.055 g/cc @Temperature 77.0 °F |
|
Indium Corp. #1010 Wave Solder Flux, Water-Soluble Wave Solder Flux #1010 is a versatile VOC-Free water-soluble wave flux that provides excellent solderability on difficult to solder assemblies. Wave Solder Flux #1010 is biodegradable and cleans to.. |