Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.014 g/cc @Temperature 25.0 °C |
1.014 g/cc @Temperature 77.0 °F |
|
Indium Corp. 1075-EX 30 VOC-Free Wave Solder Flux 1075-EX 30 is a resin/rosin-free flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075-EX 30 is a water-based, non-flammable for.. |
|||
Specific Gravity | 1.014 g/cc @Temperature 15.5 °C |
1.014 g/cc @Temperature 59.9 °F |
|
Indium Corp. 1075-EX 30 VOC-Free Wave Solder Flux 1075-EX 30 is a resin/rosin-free flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075-EX 30 is a water-based, non-flammable for.. |
|||
Specific Gravity | 1.014 g/cc @Temperature 25.0 °C |
1.014 g/cc @Temperature 77.0 °F |
|
Indium Corp. WF-7742 VOC-Free Wave Solder Flux WF-7742 is a VOC-free, no-clean flux specifically developed for Pb-free wave soldering of surface-mount, mixed technology and through-hole electronics assemblies.WF-7742 is a water-based, non-flamma.. |
|||
Specific Gravity | 1.014 g/cc @Temperature 15.5 °C |
1.014 g/cc @Temperature 59.9 °F |
|
Indium Corp. WF-7742 VOC-Free Wave Solder Flux WF-7742 is a VOC-free, no-clean flux specifically developed for Pb-free wave soldering of surface-mount, mixed technology and through-hole electronics assemblies.WF-7742 is a water-based, non-flamma.. |