Polymer Property : Specific Gravity = 1.008 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.008 g/cc

@Temperature 25.0 °C
1.008 g/cc

@Temperature 77.0 °F
Indium Corp. 1075 Wave Solder Flux VOC-Free
1075 VOC-Free is a resin-rosin-free flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075 VOC-Free is a water-based, non-flammab..
Specific Gravity 1.008 g/cc

@Temperature 15.5 °C
1.008 g/cc

@Temperature 59.9 °F
Indium Corp. 1075 Wave Solder Flux VOC-Free
1075 VOC-Free is a resin-rosin-free flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075 VOC-Free is a water-based, non-flammab..