Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.963 g/cc @Temperature 15.5 °C |
0.963 g/cc @Temperature 59.9 °F |
|
Indium Corp. 1081 Wave Solder Flux, Water-Soluble Wave Solder Flux 1081 is a water wash organic solder flux suitable for all conventional tin/lead alloys. 1081 exhibits excellent solderability with low ionic residues after aqueous cleaning.Feature.. |