Specific Gravity 0.866 g/cc

@Temperature 15.5 °C
0.866 g/cc

@Temperature 59.9 °F
Indium Corp. 1085 Wave Solder Flux, Water-Soluble
Wave Solder Flux 1085 is a water-soluble flux specifically developed for soldering surface-mount, mixed-technology and through-hole electronic assemblies.1085 is biodegradable and cleans readily in ..