Polymer Property : Specific Gravity = 0.813 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.813 g/cc

@Temperature 15.5 °C
0.813 g/cc

@Temperature 59.9 °F
Indium Corp. 3590-TX Wave Solder Flux, No-Residue
Wave Solder Flux 3590-TX is a low-solids, non-halide rosin/resin free flux designed to eliminate post-cleaning operations. Very effective flux activators provide superior solderability, reduced def..