Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.809 g/cc @Temperature 15.5 °C |
0.809 g/cc @Temperature 59.9 °F |
|
Indium Corp. 16-1081T Flux Thinner 16-1081T flux thinner is for use with Wave Solder Flux 1081-T, to maintain specific gravity during use.Physical PropertiesColor: ClearInformation provided by the manufacturer, Indium Corporation of.. |