Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.065 cm/cm | 0.065 in/in | ISO 294-4 |
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Linear Mold Shrinkage | 0.065 cm/cm | 0.065 in/in | ISO 294-4 |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |