Polymer Property : Linear Mold Shrinkage = 0.0508 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00130 - 0.0508 cm/cm
0.00130 - 0.0508 in/in
Average value: 0.0137 cm/cm Grade Count:296
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..