Physical Properties Metric English Comments
Linear Mold Shrinkage 0.03 cm/cm
0.03 in/in
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE
Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri..