Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0252 cm/cm | 0.0252 in/in | |
Plastcom SLOVALEN PQ 83 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |
|||
Linear Mold Shrinkage | 0.0252 cm/cm | 0.0252 in/in | |
Plastcom SLOVALEN PQ 53 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |