Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0250 cm/cm | 0.0250 in/in | ASTM D955 |
Niche Polymer PA66GF33BK Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.0250 cm/cm | 0.0250 in/in | ASTM D955 |
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.0250 cm/cm | 0.0250 in/in | ASTM D955 |
Niche Polymer PA66GF43N Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |