Physical Properties Metric English Comments
Linear Mold Shrinkage 0.02 cm/cm
0.02 in/in
ISO 2577
Polyram RamSter PF340S4 PBT, 20% Glass Beads
20% Glass bead reinforced PBT for injection molding applications.Information provided by Polyram Ram On Ind.