Polymer Property : Linear Mold Shrinkage = 0.0190 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0190 cm/cm
0.0190 in/in
ASTM D955
Niche Polymer PA66MIBK Nylon 66, Medium Impact
Information provided by Niche Polymer
Linear Mold Shrinkage 0.0190 cm/cm
0.0190 in/in
ASTM D955
Niche Polymer PA66MIN Nylon 66, Medium Impact
Information provided by Niche Polymer