Polymer Property : Linear Mold Shrinkage = 0.0184 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0184 cm/cm
0.0184 in/in
STN EN ISO 294-4
Plastcom PLASTALEN® PH 91 SDU Polypropylene
Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o.
Linear Mold Shrinkage 0.0184 cm/cm
0.0184 in/in
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant
FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin..