Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0178 cm/cm | 0.0178 in/in | STN 64 0808 |
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |