Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0158 cm/cm | 0.0158 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 W 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filler. Used for grips of electric hand tools, hobby tools, gear wheels, covers of electric tools, flat products, automobile wheel .. |