Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0153 cm/cm
0.0153 in/in
Plastcom SLOVAMID 6 FRC 2 LI PA6, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..