Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0147 cm/cm | 0.0147 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 FRB 4 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance. Halogen-free flame retardant. Intended for electrical purposes. Manufacturing of simple large scale products. Good flo.. |