Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0124 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
ASTM D955-95
Multibase Multi-Flex® TPO D 3105
The following is the actual data obtained from the above sample number. This material is based on new generation TPO technology. It has been designed for use as the first shot for airbag covers.Da..
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
ASTM D955
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
ASTM D955
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
STN 64 0808
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant
FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines..
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVAMID 6 FRC 3 PA6, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 for injection moulding with increased flammability resistance, with nonhalogen and phosporus flame retardant. Excellent..
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVAMID 6 FRC 2 TS PA6, flame retardant, heat stability
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..