Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® PQ 81 T 20 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 20% mineral filler. General application in all industry branches. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® T 20 Regranulate Polypropylene reinforced with mineral filler PP regranulate for injection molding with 20% mineral filler. Application for general purposes in all industrial sectors.Information Provided by Plastcom spol. s r.o. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | ASTM D955 |
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | ASTM D955 |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | ASTM D955 |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | ASTM D955 |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | |
Plastcom SLOVALEN PQ 81 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | ASTM D955 |
Plenco 2308 Phenolic, Granular, Injection Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Linear Mold Shrinkage | 0.0102 cm/cm @Thickness 4.00 mm |
0.0102 in/in @Thickness 0.157 in |
|
Azoty Tarnow™ TARNOFORM 300 GF5 POM 26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Linear Mold Shrinkage | 0.0102 cm/cm @Thickness 4.00 mm |
0.0102 in/in @Thickness 0.157 in |
|
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Linear Mold Shrinkage | 0.0102 cm/cm @Thickness 4.00 mm |
0.0102 in/in @Thickness 0.157 in |
|
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Linear Mold Shrinkage | 0.0102 cm/cm | 0.0102 in/in | 60x60x4 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |