Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00895 cm/cm | 0.00895 in/in | AMMS; ISO 2577 |
Solvay Engineered Polymers SEQUEL® 2380 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2380 engineered polyolefin is designed for large mold-in-color automotive interior applications that require stiffness and dimensional stability over a broad temperature range... |