Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.007 cm/cm | 0.007 in/in | ASTM D955 |
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |