Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°..
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
Post shrinkage is 0.26% at 72hr 120°C.; ASTM D955
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p..
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Plenco 2567 Phenolic, Granular, Injection Molded
PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo..
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Plenco 7500 Phenolic, Granular, Transfer Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Plenco 2300 Phenolic, Granular, Transfer Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Plenco 4504 Phenolic, Granular, Injection Molded
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c..