Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00480 - 0.0400 cm/cm
0.00480 - 0.0400 in/in
Average value: 0.0197 cm/cm Grade Count:97
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..