Polymer Property : Linear Mold Shrinkage = 0.0046 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0046 cm/cm
0.0046 in/in
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage 0.0046 cm/cm
0.0046 in/in
STN EN ISO 294-4
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the ..
Linear Mold Shrinkage 0.0046 cm/cm
0.0046 in/in
ASTM D955
Plenco 6527 Phenolic, Granular, Injection Molded
PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco.