Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0041 cm/cm
0.0041 in/in
ASTM D955
PolyOne Therma-Tech™ NJC-8500 Nylon 12  (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0041 cm/cm
0.0041 in/in
ASTM D955
Plenco 2567 Phenolic, Granular, Compression Molded
PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo..
Linear Mold Shrinkage 0.0041 cm/cm
0.0041 in/in
ISO 2577
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic
Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc.
Linear Mold Shrinkage 0.0041 - 0.0053 cm/cm
0.0041 - 0.0053 in/in
Annealed; ASTM D955
Dow TF0807 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow