Linear Mold Shrinkage 0.00280 - 0.00400 cm/cm

@Temperature 80.0 - 80.0 °C
0.00280 - 0.00400 in/in

@Temperature 176 - 176 °F
Average value: 0.00304 cm/cm Grade Count:20
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..