Polymer Property : Linear Mold Shrinkage = 0.00251 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00251 cm/cm
0.00251 in/in
ASTM D955
Plenco 4349 Phenolic, Granular, Compression Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..