Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00070 - 0.0017 cm/cm
0.00070 - 0.0017 in/in
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound
BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf..