Polymer Property : Linear Mold Shrinkage = 0.00160 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00160 - 0.0600 cm/cm
0.00160 - 0.0600 in/in
Average value: 0.0150 cm/cm Grade Count:136
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Linear Mold Shrinkage 0.00160 - 0.0230 cm/cm
0.00160 - 0.0230 in/in
Average value: 0.00963 cm/cm Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Linear Mold Shrinkage 0.00160 - 0.0270 cm/cm
0.00160 - 0.0270 in/in
Average value: 0.0153 cm/cm Grade Count:41
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..