Linear Mold Shrinkage 0.00020 - 0.0012 cm/cm
0.00020 - 0.0012 in/in
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester
BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced..